Unit | National Standard | Our test | Note | |
Density | kg/m3 | 10-100 | GB/T13350-2000 | |
Average fiber diameter | μm | ≤8.0 | 5.5 | GB/T13350-2000 |
Hydrophobic rate | % | ≥98 | 98.2 | JISA9512-2000 |
Thermal Conductivity | w/m.k | ≤0.042 | 0.033 | GB/T13350-2000 |
Incombustibility | 0 | Non-flammable | Non-flammable | GB/T13350-2000 |
Sound absorption coefficient | 0 | 0 | 1.03 Product reverberation method 24kg/m3 2000HZ | GB/J47-83 |
High temperature | ℃ | 400 | 410 | GB/T13350-2000 |